We use cookies to enhance your browsing experience, serve personalized ads or content, and analyze our traffic. By clicking "Accept All", you consent to our use of cookies. Read more about privacy policy.

Perkin Elmer DSC8500 Differential Scanning Calorimeter with Polyscience VLT-100 Cooling Unit and software

Perkin Elmer DSC8500 Differential Scanning Calorimeter with Polyscience VLT-100 Cooling Unit and software

Contact us for price

Description

The PerkinElmer DSC 8500 (Differential Scanning Calorimetry) features second-generation HyperDSC technology, which allows you to gain unlimited insight into the structure, properties and performance of your materials. And with hyper-enabled, double-furnace technology and better application capabilities, the DSC 8500 gives you higher accuracy and sensitivity than ever before.

Typical applications for the DSC 8500:

  • Polymorph characterization in pharmaceuticals
  • Measure samples without heating induced polymorph changes
  • Process studies in pharmaceuticals
  • Get a greater understanding of how the process affects the amorphouscrystalline content of the product
  • Process simulation in polymers
  • See the effects your process has on the product

Features: 

  • Double-furnace DSC
  • HyperDSC
  • Enhanced software package
  • 96-position autosampler
  • Extremely fast controlled scanning rates to 750 °C/min
  • In-situ ballistic cooling to 2100 °C/min, enabling experiments that mimic real-world processes
  • Extremely fast readout rates (100 points/second) providing high data integrity
  • Proven HyperDSC superiority in:
  • Isothermal crystallization
  • Polymorph/amorphous-material studies
  • High sensitivity measurements
  • Process simulation

Specifications

  • Dimensions (without autosampler): 21″ W x 24″ D x 12″ H (20 x 54 x 62 cm)
  • Dimensions (with autosampler): 21″ W x 24″ D x 20″ H (54 x 62 x 50 cm)
  • Weight (without autosampler): 44 lb (20 kg)
  • Weight (with autosampler): 66 lb (30 kg)
  • Power: 100-240 Volt, 50/60 Hz

Calorimetric Performance

  • Dynamic range of ±1300 mW allows applications with high energy thermal transitions to be measured
  • Accuracy: <±0.2%
  • Precision: <±0.03%
  • Indium height/width (mW/°C) 18.4. Indium melting peak height/width at half-height. 1 mg
  • Indium, 10 °C/min, nitrogen purge. No mathematical treatment to the data or correction applied.
  • Indium melting time (sec) 2.3. The time between Indium melting peak onset and maximum.

Temperature Performance

  • Range: -180 °C to 750 °C
  • Accuracy ±0.05 °C using on-set temperatures of Indium melting peak
  • Precision ±0.008 °C
  • Data points/sec: 100
  • Controlled heating rates: 0.01 to 750 °C/min
  • Controlled cooling rates: 0.01 to 750 °C/min – depends on cooling accessory installed and cooling range selected
  • In-situ ballistic sample cooling of up to 2100 °C Included
  • Between-sample cooling times (100 to -100 °C with CLN2 cooling accesory): 30 seconds

Controlled Cooling 

  • Ambient coolant – nitrogen purge:
  • 10 °C/min to 22 °C
  • 20 °C/min to 35 °C
  • 50 °C/min to 70 °C
  • 100 °C/min to 125 °C
  • Liquid N2 coolant – helium purge:
  • 10 °C/min to -170 °C
  • 50 °C/min to -165 °C
  • 100 °C/min to -140 °C
  • 200 °C/min to -100 °C
  • 300 °C/min to -60 °C
  • 400 °C/min to -20 °C
  • 500 °C/min to 30 °C
  • 750 °C/min to 100 °C


Specifications

ManufacturerPerkin Elmer
ModelDSC8500 Differential Scanning Calorimeter with Polyscience VLT-100 Cooling Unit and software
ConditionUsed
Stock NumberBM5561